Paint film questions/problems after the paint film totally dried:

30. Orange peel - the paint looks like the orange surface, and is not even;

31. Wave marks - when observe the paint film from certain distance, the paint film looks like the wave;

32. Wiredrawing - paint film surface appears like hair type filiform;

33. Fisheye/shrinkage hole - paint film surface appears small holes;

34. Poor adhesion - paint film is easily peeled from substrate;

35. Paint film tendering

36. Partides - there are partides on paint film;

37. Biting - the spraying layer "bites" preceding coats;

38. Shrinking - paint surface problem;

39. Gloss losing - paint film lose gloss after certain period;

40. Cracking - crackles appears in the paint film;

41. Hazing - when spraying basecoat to be the paint film, color of film is not even;

42. Water marks - differents shapes of marks appears on paint film, color inside mark is lighter than main color;

43. Gloss shrinking - paint film is half hazing, sometimes, sanding marks appears on paint film;

44. Bubbles - there are many bubbles during paint film drying time;

45. Sand paper marks - sand paper marks and other marks appears after paint film dried;

46. Paint film not dried well - too short drying time or cannot be dried totally, paint film is soft, low hardness, poor adhesion;

47. Paint film soft - paint film is easily having scratches;

48. Cloudy - cloudies on paint film surface;

49. Dizziness - there are dizzy circles on paint film;

50. Different people color variance - after the paint film be dried, one engineer eye-check color with standard color panel, deciedes it is fine; but another engineer eye-check it, finds color is not match standard color panel;

51. Eye-checking color variance - check color by eyes, finds color variance;

52. Instrument-checking color variance - check color by color variance instrument, finds color variance;

53. What color variance is scientific for solids colors?

54. What color variance is scientific for silver colors?

55. There is always paint film crackes in areas of different materials attaches, how to handle it?

【Back】
Shanghai Downtown Office:D72-74 No 313 Xiuyan Road Pudong Shanghai   Postcode:201315
Tel:86 21 2092 9081, 2092 9082, 2092 9083 Fax: 86 21 209 29080
Technical Service Center: Floor 6, No. 2 Building, No. 4777, Jiasong Bei Road, Shanghai   Postcode:201814   Tel:59506133
Copyright © 2010 Shanghai LXZXL Chemical Co., Ltd Technical support:China Network Services   SMS